J.Leclair
Well-Known Member
Here's my next 3 knives ground ready for Pin holes and pre HT hand sanding to fix a couple small wobbles in the grind lines. I wanted to try to make 3 knives from the same template but do each one a bit different from the next.
All are 10" OAL with 5" Blades
Top one is an almost full height hollow grind from 1/8" 440c
Middle one is about a 2/3 height hollow grind from 1/8" 440c added a swedge to this one.
Bottom one is also a 2/3 height hollow grind this one is from 3/16" 440c this one also has a swedge but gave this one a subtle recurve.
I want to try bolsters for the frist time on one of them, most likely the first one. I have some 1" x 3/4" nickle silver bar stock with pins of the same
comments or critiques welcomed and encouraged.

All are 10" OAL with 5" Blades
Top one is an almost full height hollow grind from 1/8" 440c
Middle one is about a 2/3 height hollow grind from 1/8" 440c added a swedge to this one.
Bottom one is also a 2/3 height hollow grind this one is from 3/16" 440c this one also has a swedge but gave this one a subtle recurve.
I want to try bolsters for the frist time on one of them, most likely the first one. I have some 1" x 3/4" nickle silver bar stock with pins of the same
comments or critiques welcomed and encouraged.