I had one of those 'I wonder what it would be like' ideas and tried making a full stainless friction folder. Normally I grind AEB-L after the heat treat, but this time I tried it before. It's going to be a rough looking 'industrial' kind of finish so the blade wasn't taken to a very high polish. It's definitely not my best grind either. Although it takes longer to grind, I think I like grinding post heat treat. 1/2" holes to put the size in perspective.