Last year my Brother in Law (16y o) came to the house and did a small fixed blade with CF and 110WCRV. That year as we haven't enough time to make a folder, he did a niolox and g10 fixes blade.
I drawned some schemed and that one was the he wanted to do. Cut of the paper, inked of the steel and draw on the steel.
Band saw time for the steel and g10
The grind is completed with backstand
Bevel Grind
Some small hole
Is it OK?
Hardening
Toxification
During the gluing time, i make him do a small pendent in snakewook for his girl friend
And the knife he has done. He did almost everything, i cleaned just a bit the grind and did the quench.
Sharp 8 cm for 19 cm long.

I drawned some schemed and that one was the he wanted to do. Cut of the paper, inked of the steel and draw on the steel.


Band saw time for the steel and g10

The grind is completed with backstand

Bevel Grind

Some small hole

Is it OK?

Hardening

Toxification



During the gluing time, i make him do a small pendent in snakewook for his girl friend







And the knife he has done. He did almost everything, i cleaned just a bit the grind and did the quench.
Sharp 8 cm for 19 cm long.