I ordered some 1095 from USAknifemaker. Three 12" lengths. I used 2 of the lengths to make knives already. After the heat treat I noticed they had warped pretty severely, which I found odd because I never seem to have a problem with it especially with stock removal and properly annealed steel from reputable companies. I managed to get them straight enough for my knife and my buddies knife, but they aren't perfect. I always leave more than a dimes width of stock on the edge prior to heat treat just to be sure, and I used the "shimming with a penny during temper" method to straighten them.
This past weekend, I was working on a third knife with this last piece of 1095. I had a hard time getting the flat grind straight on one side. I look down the spine and it's already warped like crazy from tip to butt. I realized the 2 others where probably the same. Why I'm just now checking for straightness before grinding...just call it inexperience.
I guess I'm making this thread because I've never noticed this to be a problem when ordering steel in smaller lengths like this and I need to ask how you deal with it.
Would it be better to try and hammer it out right now before heat treat or wait and try to correct later? Is it ok to stick it in the over at around 300 and try the shim thing now, before heat treat? What methods do you use?
This past weekend, I was working on a third knife with this last piece of 1095. I had a hard time getting the flat grind straight on one side. I look down the spine and it's already warped like crazy from tip to butt. I realized the 2 others where probably the same. Why I'm just now checking for straightness before grinding...just call it inexperience.
I guess I'm making this thread because I've never noticed this to be a problem when ordering steel in smaller lengths like this and I need to ask how you deal with it.
Would it be better to try and hammer it out right now before heat treat or wait and try to correct later? Is it ok to stick it in the over at around 300 and try the shim thing now, before heat treat? What methods do you use?